With regard to the RW at 450 °C, the cured resin generally exhibited an increasing trend with increasing DAS, indicating an improvement in the thermal stability of the modified resins.
← all excerpts
Toughening and Enhancing Melamine-Urea-Formaldehyde Resin Properties via in situ Polymerization of Dialdehyde Starch and Microphase Separation.