In 3 hours of ultrasonic treatment, the tensile properties displayed an increasing trend prior to decreasing trend as the GNP increased from 0 to 2 wt.% ( Fig 1(B)) .
← all excerpts
Enhanced mechanical and thermal properties of electrically conductive TPNR/GNP nanocomposites assisted with ultrasonication.