Differences between groups of *p < 0.05 were considered statistically significant, **p < 0.01 were considered highly significant. 3 Results 3.1 The PTA scaffold prepared for in vivo implantation PTA was dissolved in 1,4-dioxane and PTA scaffold was prepared by the thermal-induced phase separation technique ( Fig. 1 A).
← all excerpts
Photoluminescent biodegradable polyorganophosphazene: A promising scaffold material for <i>in vivo</i> application to promote bone regeneration.