With the increase of the annealing temperature, the strength keeps decreasing, while the elongation shows an increasing trend at the beginning and then a decreasing trend after the peak of 32.5% (annealed at 350 °C).
← all excerpts
Effect of Annealing on the Interface and Mechanical Properties of Cu-Al-Cu Laminated Composite Prepared with Cold Rolling.