At the same time, the content of C 2 S and C 3 A shown a decreasing trend, while the amorphous content shown a rising trend.
← all excerpts
Effects of Calcination Conditions on the Formation and Hydration Performance of High-Alite White Portland Cement Clinker.
2
—
—
The sentences
From Figure 12 , it was noted that, with the increase of sintering temperature (1450~1525 °C), the total heat release presents an increasing trend, but for the sintering time (60~240 min), the total heat release is ranked from high to low as follows: 60 min→120 min→240 min→180 min.