Longer UV exposure of oxo-LDPE samples, for 758 and 900 h, showed a decreasing trend in CO 2 evolution compared with that observed after 450 h.
← all excerpts
Microbial Degradation of Plastic in Aqueous Solutions Demonstrated by CO<sub>2</sub> Evolution and Quantification.