The highest flexural strength shows a decreasing trend of NCC > CNTs > nano-SiO 2 at both 7 d and 28 d, and the intensity of the CNTs group changes with the dosage is larger than that of the nano-SiO 2 and NCC groups.
← all excerpts
A Comparative Study on the Effects of Three Nano-Materials on the Properties of Cement-Based Composites.
2
—
—
The sentences
The water absorption rate ranking of the CNTs group is 0.1% < 0.01% < 0% < 0.5% < 2% < 3%, an overall trend which is the opposite of the compressive strength one, indicating that CNTs also have a good filling effect on the internal pores of mortar specimens.