In Figure 5 b and Table 3 , the elongation at break of SSBR/PPD-GO composites was almost equivalent to that of SSBR, which showed a slight trend of increasing first and decreasing later.
← all excerpts
Effect of Graphene Oxide Modified with Organic Amine on the Aging Resistance, Rolling Loss and Wet-skid Resistance of Solution Polymerized Styrene-Butadiene Rubber.