This is a highly significant result because the oxide solid electrolyte has low ionic conductivity 47 and it is difficult to operate an oxide ASSB at room temperature 48 owing to the formation of a heterogeneous layer at the interface between the solid electrolyte and the active electrode material during the calcination process 49 .