The benefits may be significant if one compares the properties for hot processed alloy Zn-0.5 Mg [ 7 ] with cold HE method, see Chapter 3.13., Table 2 , UTS = 300 vs. 515 MPa, YS = 160 vs. 375 MPa and 65 HV vs. 105 HV, or for the Zn–1Mg alloy: UTS = 340 vs. 480 MPa, YS = 180 vs. 365 MPa, ε f = 6 vs. 25% and 75 HV vs. 110 HV.
← all excerpts
Structural and mechanical aspects of hypoeutectic Zn-Mg binary alloys for biodegradable vascular stent applications.
1
—
—