The near-surface hardness of the samples processed with S10 had an increasing trend depth between 20–70 μm, whereas that of the samples modified with S60 had a slight decreasing trend in the SPD zone ( Figure 4 ).
← all excerpts
Surface, Subsurface and Tribological Properties of Ti6Al4V Alloy Shot Peened under Different Parameters.