While the hydrolytic degradation results match those of previous studies, wherein SMP foams were stable over 36 weeks of testing in 0.1 M NaOH [ 20 ], these results are highly significant when taken with previous oxidative testing results.
← all excerpts
Shape Memory Polymer Foams Synthesized Using Glycerol and Hexanetriol for Enhanced Degradation Resistance.