In the groups with a higher concentration of HEMA (resins 4 to 6), a decreasing trend with an increase of BisGMA fraction and thus also viscosity of the adhesive was observed ( DC POSS4 = 56.4%, DC POSS5 = 17.1%, DC POSS6 = 9.6 %).
← all excerpts
Characterization of Methacrylate-Based Resins Containing Methacryl-Polyhedral Oligomeric Silsesquioxanes (MA-POSS-8).