When dopant amounts were increased from x = 0.02 to x = 0.08, there was an increasing trend of grains sizes formation in the compounds.
← all excerpts
Understanding the structural, optical, and dielectric characteristics of SrLaLiTe<sub>1-x</sub>Mn<sub>x</sub>O<sub>6</sub> perovskites.