At 920 °C, the conversion rate increased until H 2 O/CO 2 ratio was 0.15, and in cases where H 2 O/CO 2 ratio was greater than 0.15, it showed a decreasing trend.
← all excerpts
The effect of H<sub>2</sub>O on the sulfation of Havelock limestone under oxy-fuel conditions in a thermogravimetric analyser.