Between 1200 and 1750 nm, attenuation follows a decreasing trend proportional to λ −5 .
← all excerpts
Performance Study of a Zirconia-Doped Fiber for Distributed Temperature Sensing by OFDR at 800 °C.
1
—
—
Between 1200 and 1750 nm, attenuation follows a decreasing trend proportional to λ −5 .