Experimental drug loading on the other hand, ranged between 0.11 and 7.15% ( Table 2 ), with an increasing trend following the increment of the initial amount of A/S mixture used for the preparation of the samples.
← all excerpts
Novel electrospun poly-hydroxybutyrate scaffolds as carriers for the wound healing agents alkannins and shikonins.
2
—
—
The sentences
The porosity factors of the electrospun A/S mixture-loaded PHB scaffolds fabricated in this study are shown in Table 2 , where a decreasing trend can be seen, following the increment of the initial amount of A/S mixture used for the preparation of the samples.