A decreasing trend in the intensity of the O–H transmittance band at 3450–3400 cm −1 indicated that the hydroxyl group content in the treated fibers were reduced after the T2 treatment.
← all excerpts
Effect of Rot-, Fire-, and Water-Retardant Treatments on Jute Fiber and Their Associated Thermoplastic Composites: A Study by FTIR.