When the ultrasonic amplitude was increased from 20 to 100%, the specific surface area of the vaterite samples showed an increasing trend and rapid enlargement, from the initial value of 12.27 to 20.91 m 2 /g at a probe immersion depth of 60 mm and a solution volume of 180 mL.