No matter what the temperature we choose, RBER has an initially higher value at the fresh state with a decreasing trend in sub-200 P/E cycles, and then it increases during subsequent P/E cycling.
← all excerpts
Temperature Impacts on Endurance and Read Disturbs in Charge-Trap 3D NAND Flash Memories.