A decreasing trend with lower results after aging, when an adhesive system is tested after long-term storage in dentin, is not only expectable but certain, due to enzymatic and hydrolytic degradation [ 42 , 66 , 67 ].
← all excerpts
Investigating a Commercial Functional Adhesive with 12-MDPB and Reactive Filler to Strengthen the Adhesive Interface in Eroded Dentin.
3
—
—
The sentences
Although no significant differences were found between mean μTBS values, for different adhesives and time points ( p > 0.05), a positive trend, with μTBS rising in the CFP_3M group, was observed.
No significant differences were found between the experimental groups at different time points, as evidenced by two-way ANOVA ( p = 0.087), although an increasing trend was noted in the CFP_3M group.