In addition, the sheet resistance of the LIG demonstrated a decreasing trend from 51.6 ± 2.0 Ω sqr –1 (LIG30%) to 36.9 ± 2.6 Ω sqr –1 (LIG60%) with the increase of laser power over the range of 30–60%, while a further increase of laser power led to an apparent increase in sheet resistance to 55.8 ± 1.4 Ω sqr –1 (LIG100%).
← all excerpts
Conducting Polymer-Reinforced Laser-Irradiated Graphene as a Heterostructured 3D Transducer for Flexible Skin Patch Biosensors.