[ 20 ] also observed a decreasing trend in the value of the compressive strength of clay–tuff samples manufactured by extrusion at temperatures up to 1050 °C, obtaining compressive strengths up to 23MPa.
← all excerpts
Volcanic Tuff as Secondary Raw Material in the Production of Clay Bricks.
2
—
—
The sentences
Even though the energy used for brick production has been reduced since 1990 [ 2 ], the role of industry in transitioning to climate neutrality [ 3 ] may be significant.