† For 1–8 ML G-ZnO, strain shows an increasing trend as the thickness increases, indicating that E ads (the red line in Fig. 2B ) shows a scaling relationship with the strain (Fig.
← all excerpts
Achieving flexible large-scale reactivity tuning by controlling the phase, thickness and support of two-dimensional ZnO.