For Ti6Al4V tested in Hanks’ solution with an added mixture of LA and H 2 O 2 , the open circuit potential value shows a decreasing trend in the first 3 h from 406.78 mV vs.
← all excerpts
Reactivity and Corrosion Behaviors of Ti6Al4V Alloy Implant Biomaterial under Metabolic Perturbation Conditions in Physiological Solutions.
2
—
—
The sentences
From the EDX spectra and chemical analysis of Ti6Al4V alloy surface immersed in Hanks’ solution with added mixture of lactic acid and an inflammatory compound, a decreasing trend of mass percentage of Ti element to 78.89%, an increasing trend of oxygen element to 8.77% and the apparition of carbon element at 4.17% can be seen.