As the magnetic fields increase, the ΔS−T curve changes from the symmetrical herringbone to the asymmetric curve, indicating that the alloy phase transition type from the secondary phase transition to the primary phase transition and ΔS shows an increasing trend (because the primary phase transition is the change of material magnetic ordered state caused by lattice distortion, the resulting magnetic entropy change is much greater than the secondary phase transition and reaches values of 9.45 J/(kg·K) upon an applied field of 1.5 T). 4.
← all excerpts
Microstructure and Magnetocaloric Effect by Doping C in La-Fe-Si Ribbons.
2
—
—
The sentences
The maximum isothermal magnetic entropy change mutated after 20 min of heat treatment, and then showed an obvious trend of first increasing and then decreasing, and reached the maximum value after 2 h of heat treatment.