Analyzing the average G II fold change values ( Figure 7 D), there is, once again, a positive trend by increasing the rubber content.
← all excerpts
Self-Assembled NBR/Nomex Nanofibers as Lightweight Rubbery Nonwovens for Hindering Delamination in Epoxy CFRPs.
2
—
—
The sentences
Comparing these results with previously reported nanomodified CFRPs with NBR/PCL nanofibrous mats, 21 it is evident that the enhancement is less pronounced (up to +180 vs +480%) but still highly significant.