In general, an increasing trend in YM was observed over time and 16 days after CTH samples were determined to have similar values relative to samples that were not damaged.
← all excerpts
Fluorescent Ionic Probe for Determination of Mechanical Properties of Healed Poly(ethylene-<i>co</i>-methacrylic acid) Ionomer Films.