It is worth mentioning that the activation energy and the stack structure parameters have a sharp transition at 300 °C, and the activation energy has the same increasing trend with the effective stacking height (Lc) and stacking layer number (n), but the opposite trend with an increasing trend of aromatic layer spacing (d 002 ).
← all excerpts
HRTEM analysis of the aggregate structure and ultrafine microporous characteristics of Xinjiang Zhundong coal under heat treatment.