After loading Cu x O, the surface areas of catalysts present an initial increase and then a decreasing trend in the range of 260–290 m 2 g −1 , among which Cu1.0 achieves the largest surface area (289.5 m 2 g −1 ).
← all excerpts
Generation of multi-valence Cu <sub><i>x</i></sub> O by reduction with activated semi-coke and their collaboration in the selective reduction of NO with NH<sub>3</sub>.