The pore size distributions indicate that the pores of the AMA and NAMA catalysts were in the mesoporous range (20–500 Å), and results show a decreasing trend from 50 to 40 Å with an increase in Mo loading from 6 to 12 wt%.
← all excerpts
Epitaxial synthesis of Ni-MoS<sub>2</sub>/Ti<sub>3</sub>C<sub>2</sub>T <sub><i>x</i></sub> MXene heterostructures for hydrodesulfurization.