Furthermore, as summarized in Table 1 , the surface area of the composite membranes increased from 18.5 to 26.8 m 2 g −1 after adding the CD and CTA into the electrospinning solution, whereas the pore size showed a decreasing trend due to the embossments formed on the nanofibers.