As shown in Table 3 , when DAC feed ratio was 30%, [ η ] of TPADs (TPAD1–TPAD4) showed an increasing trend with the increase in the amount of TiO 2 , reaching the maximum value at TiO 2 content (0.250 wt‰) and then slightly decreased.