Furthermore, the T lum,l and T lum,h of these samples both increased obviously as the refractive indices of SiO 2 coatings increased from 1.16 to 1.42, and the values of Δ T sol also exhibited a slightly increasing trend at the same time.
← all excerpts
Enhanced visible transmittance and reduced transition temperature for VO<sub>2</sub> thin films modulated by index-tunable SiO<sub>2</sub> anti-reflection coatings.