SEM observation shows that the average particle size of carbonate precursor exhibits a decreasing trend with the reactant concentration, and the one synthesized at 0.3 mol L −1 has relatively smaller particle size with more homogenous distribution.
← all excerpts
Urea-assisted hydrothermal synthesis of a hollow hierarchical LiNi<sub>0.5</sub>Mn<sub>1.5</sub>O<sub>4</sub> cathode material with tunable morphology characteristics.