The elevated ridges were reduced when a low VED (63 J/mm 3 ) was used for melting the last layer, and generally had a decreasing trend with increasing the hatch angle rotation and the number of the last layers melted.
← all excerpts
Investigation of Scanning Strategies and Laser Remelting Effects on Top Surface Deformation of Additively Manufactured IN 625.