Effect of Lanthanum Oxide Addition on Microstructure and Wear Performance of Iron-Chromium Alloy Manufactured by Laser Direct Deposition Additive Manufacturing.

Materials (Basel) · 2022 · PMC9100016 · PMID 35591568

2
hedged sentences
closest p
boldest claim

The sentences

a decreasing trendno p-value reported
As the mass fraction of La 2 O 3 increases, the depth and width of the groove show a decreasing trend.

also in 47,180 other papers

an increasing trendno p-value reported
The worn surface topography of each sample shown in Figure 11 verifies that, as the mass friction of La 2 O 3 increases, the wear resistance and wear reduction of AM alloy show an increasing trend.