By comparing the pristine composite series cured at 150 °C, 160 °C, and 190 °C, the tensile strength increased as the curing temperature increased, and we recorded a decreasing trend with the increased amount of FA incorporated into the rubber-plastic-wood blend.
← all excerpts
The Influence of Fly Ash on the Mechanical Properties of Water Immersed All Waste Composites.
2
—
—
The sentences
The compressive strength of the pristine series registered an increasing trend as a small fly ash amount was added to the rubber-PET-HDPE-wood blend, Figure 2 .