The compressive strength of MF/SiC NWS showed a decreasing trend with increasing test temperature, but when the test temperature increased to 1400 °C, the compressive strength of MF/SiC NWS was still up to 0.45 Mpa, with strength retention of 96%, indicating its excellent thermal stability in high temperatures. 4.