However, no statistical differences were reported after subsequent deposition of 4 and higher numbers of bilayers (thickness: LbL4_dip = 37.88 ± 2.54 nm; LbL7_dip = 40.15 ± 4.08 nm; LbL10_dip = 35.68 ± 5.90 nm), whose average heights did not follow an increasing trend with the number of dipping cycles ( Figure 1 a).