highly significantp < 0.001
The Young’s modulus values were less dispersed in late-mature enamel ( Figure 4E ) than in early maturation ( Figure 4D ), with a highly significant difference for more mineralized late-mature enamel ( p < 0.001 ) of DEHP-treated mice.