However, the elongation at break of the PEVA composite showed a decreasing trend with increased dolomite loading.
← all excerpts
On the Use of Dolomite as a Mineral Filler and Co-Filler in the Field of Polymer Composites: A Review.
2
—
—
The sentences
Results indicated that the tensile strength, modulus of elasticity, and tensile toughness of the PEVA/dolomite composite showed an increasing trend when the dolomite content increased from 1 to 5 wt%.