highly significantp < 0.001
As per the results of roughness parameters and SEM photomicrographs of the present study, it is quite evident that 4% acetic acid was the most damaging immersion medium and produced a highly significant surface roughness of the evaluated ceramic in all dimensions ( p < 0.001), when compared to the other groups.