Nonetheless, as shown in Table 3 , the maximum decomposition temperature (T max ) and onset decomposition temperature (T 10% ) of T-LNPs exhibited an increasing trend with the increase in SA, since the phenolic hydroxyl groups from SA could trap the free radicals generated during pyrolysis, and therefore, significantly retard their degradation [ 47 ]. 3.2.