Moreover, although the compressive strengths of specimens L-5 (60% PC and 40% GBFS, 200 g LSS, Figure 1 a) and L-6 (60% PC and 40% GBFS, 300 g LSS, Figure 1 a) still followed an increasing trend, the range of the increase gradually decreased with further increase in LSS content.
← all excerpts
Coagulation Mechanism and Compressive Strength Characteristics Analysis of High-Strength Alkali-Activated Slag Grouting Material.