(2) The strain rate sensitivity of 316L exhibits an interesting trend, in that it is generally low (0.1–0.2) at 700–900 °C but increases to 0.33, at 45% strain at 1000 °C.
← all excerpts
Reveal the Viscoplastic Behaviour and Microstructure Evolution of Stainless Steel 316L.
2
—
—
The sentences
However, at 1000 °C, there is an increasing trend for the strain rate sensitivity, which increased from 0.15 at a strain level of 20% to 0.33 at a strain level of 45%.