In addition, when the amount of MMT was at 3 wt%, the tensile strength and Young modulus exhibited an increasing trend.
← all excerpts
Characteristics and performance studies of a composite polymer electrolyte membrane based on chitosan/glycerol-sulfosuccinic acid modified montmorillonite clay.
2
—
—
The sentences
However, when the concentration of MMT was at 5 and 15 wt%, the tensile strength and Young modulus exhibited a decreasing trend.