For example, increasing the PEO content from 10 to 20 wt % showed a decreasing trend of tensile modulus for PL70/PA30 from 1167 to 1017 MPa and 946 MPa for the ternary systems attributed to the substitution of the rigid components (PLA and PA11) with a soft rubbery component (PEO) of low rigidity.
← all excerpts
Biosourced Poly(lactic acid)/polyamide-11 Blends: Effect of an Elastomer on the Morphology and Mechanical Properties.