Compared with the virgin asphalt binder, the indicator m/S @ 60th increased with conditioning duration and pore water pressure magnitude, and their percent change ratios also exhibited an increasing trend, as shown in Figure 12 , which indicates a more severe erosion effect in a harsh dynamic pore water pressure environment.
← all excerpts
Rheological Behaviors and Damage Mechanism of Asphalt Binder under the Erosion of Dynamic Pore Water Pressure Environment.