The outcomes clearly demonstrate that the flexural strength was enhanced significantly or highly significant for the strengthened beams compared to the reference beams Figure 7 demonstrates that after 28 days of curing, the flexural strength enhanced by 12.42%, 20.26%, and 34.64% for the beams strengthened at 1-side, 2-sides, and 3-sides, respectively, compared to the control beams.
← all excerpts
Effect of Non-Woven Polyethylene Terephthalate (PET) Tissue on Fresh and Hardened Properties of Concrete.